Dnia 2026-05-12 o godzinie 13:15 w sali 2011 Wydziału Fizyki UwB, odbędzie się seminarium na którym Dr. Apostolos Vagias z Institut Max von Laue - Paul Langevin (ILL), Grenoble, France wygłosi wykład pt
Basic aspects of neutron science and soft matter/ infrastructures at the Institute Laue Langevin (ILL) - Polymer compatibility on mixed brushes probed by high pressure GISANS (HP-GISANS) and reflectivity
Serdecznie zapraszamy
Tomasz Karpiuk
Andrzej Maziewski
Basic aspects of neutron science and soft matter/ infrastructures at the Institute Laue Langevin (ILL) - Polymer compatibility on mixed brushes probed by high pressure GISANS (HP-GISANS) and reflectivity
dr. Apostolos Vagias
Institut Max von Laue- Paul Langevin (ILL), 71 Avenue des Martyrs, 38042 Grenoble, France
In the first part of my talk, I will cover basic aspects about neutron scattering for soft matter systems. I will then present an overview of the Large Scale Structures Group at the Institute Laue - Langevin (ILL). In the second part, I will focus on my own research background concerning supported soft matter using neutron methods under ambient and extreme conditions (high hydrostatic pressure and temperature). Background: The elucidation of material nanostructure under elevated pressures is quite relevant for devices used in deep sea research, including tactile sensors and soft robotics [1]. To accommodate resistance to harsh underwater environments, multicomponent systems need to be utilized with orthogonal properties. Technical challenges had so far hampered the investigation of thin film nanostructures of varying compositional complexity under elevated hydrostatic pressures. Methods: By utilizing a custom-made pressure cell [2] and performing Grazing Incidence Small Angle Neutron Scattering under pressure (HP - GISANS) at D22 and neutron reflectometry (NR) at FIGARO instruments of the ILL [3,4], I compare effects of pressure and temperature at the solid-liquid interface between two homopolymer mixed brushes in thin (< 100 nm) film using D2O solvent: A weakly incompatible (poly(methyl methacrylate) / poly(2-(dimethylamino)ethyl methacrylate)) (PMMA / PDMAEMA) and strongly incompatible ((poly((2,2,3,3,4,4,5,5-octafluoro)pentyl methacrylate))/ poly(2-(dimethylamino)ethyl methacrylate) ) (POFPMA/PDMAEMA) mixed brush. Results: Distinct pressure-dependent response in lateral (HP - GISANS) and transversal (specular NR) nanostructure is recorded depending on the chemical compatibility between the polymers. GISANS simulations indicate buried hydrophobic dimple-like patches within a PDMAEMA-based swollen matrix. Specular ToF-NR suggests that temperature effects are counteracted by pressure. Off-specular NR reveals large (>100 nm) lateral domains associated to the hydrophilic PDMAEMA compound, being both pressure-dependent and polymer-compatibility dependent.
Conclusion: Length scale of phase separation strongly depends on the compositional variation in the flat mixed brushes. Also, non-idealities of mixing are polymer-compatibility dependent as evidenced by enhanced D2O retention within the brush by the more strongly incompatible POFPMA/PDMAEMA.
W ramach naszego serwisu www stosujemy pliki cookies zapisywane na urządzeniu użytkownika w celu dostosowania zachowania serwisu do indywidualnych preferencji użytkownika oraz w celach statystycznych. Użytkownik ma możliwość samodzielnej zmiany ustawień dotyczących cookies w swojej przeglądarce internetowej. Więcej informacji można znaleźć w Polityce Prywatności Uniwersytetu w Białymstoku. Korzystając ze strony wyrażają Państwo zgodę na używanie plików cookies, zgodnie z ustawieniami przeglądarki.